Home > News > Content

Production Process Of Lightweight High Alumina Bricks

Nov 19, 2026

Lightweight high alumina bricks are important insulation materials for thermal furnaces. The rational manufacturing and selection of lightweight high alumina bricks are of great significance for the rational utilization of energy and the correct implementation of China's energy policies. Among various lightweight insulation materials, lightweight high alumina bricks have high fire resistance and low bulk density; Abundant raw materials and affordable refractory bricks make them ideal insulation materials. According to different manufacturing processes? Lightweight high alumina brick can be made by foam method or adding figure method.

1. Production process of lightweight high alumina brick by foam method

We use heavy-duty high alumina alumina cylindrical powder with an Al2O3 content of about 55% and combined clay fine dressing with an Al2O3 content of 31-32% as raw materials. The ratio of high alumina bauxite clinker to bound clay fine powder is 9:1. Add 48-50% water and grind in a ball mill for 1-2 hours. The slurry passes through a 0.2mm sieve with a specific gravity of 1.7-1.9 and a pH value of 7. Sodium rosinate was used to prepare foam agent. Sodium rosinate foam is made by saponifying rosin and alkali, and adding bone glue solution as stabilizer.

2. Combustible additive method

The method of adding combustible substances to clay can also produce lightweight refractory bricks with a bulk density of 0.8. The combustible additives used in production include sawdust, rice husks, coke powder, smokeless coal, etc. The requirements for combustible additives are easy to burn out, low ash content, and low levels of harmful impurities in the ash. Generally, sawdust and rice husks are used, with a dosage of 30-40%. Sawdust needs to be sieved; Rice husks can be ground together with high alumina bauxite. The mud material and combustible additive are mixed in a wet mill for 4-5 minutes, or extruded into mud strips by a screw extruder. The moisture content of the clay is 40-50%.

The mixed clay can be molded into wooden models. The wooden model is first soaked in water, brushed with sawdust, then filled with mud, scraped flat, and demolded. After drying, the blank is fired at the required temperature.

 

 

 

 

 

 

 