Ceramic roller bars operate under high temperature and load for extended periods, so various faults tend to occur during production, such as mid section breakage, thermal cracking during replacement, end cracking and bending inside the kiln. Most of these issues result from the service life of roller bars, while some are caused by inherent product defects or improper operation. A brief explanation is given below.
1. Mid section breakage of ceramic roller bars appears as transverse fracture with neat and porous fracture surfaces, also known as transverse cracking. The primary cause is operation beyond temperature limits. Different grades have maximum service temperatures: medium temperature type ≤1000℃, medium high temperature type ≤1200℃, high temperature type ≤1250℃. Exceeding these limits greatly increases the risk of breakage. Working parameters also matter. When firing large size tiles, heavier products, wider kiln spans and faster rotating speeds raise the fracture risk. Improper selection leads to failures as well. Φ50 mm roller bars are preferred for tiles above 600mm×600mm, while Φ60 mm or Φ65 mm bars suit tiles of 800mm×800 mm and larger. Ultra high temperature roller bars are required for heavy load applications including daily ceramics and rare earth calcination loaded in saggers.
2. Thermal cracking during roller bar replacement features long axial cracks, fragmentation into multiple pieces, irregular and smooth fracture surfaces. The replacement temperature should not exceed 800–850℃. Large diameter roller bars have poorer thermal stability; temperature difference stress from rapid heating and cooling easily triggers cracking. Operational mistakes are another key factor. Hot roller bars crack from local rapid shrinkage if they contact ironwork, pooled water or forced cold air. Coated roller bars that are not fully dried will crack sharply when moisture vaporizes rapidly at high temperature.
3. End cracking and breakage are mostly related to assembly and transmission fit. Mismatched tolerances between the outer diameter of the roller bar and the inner diameter of the drive sleeve, or undersized sleeves, will crack the bar end due to excessive fitting tightness. Deformed sleeves, shifted kiln walls and block bricks cause asynchronous rotation and twist off the roller bar. Excessive force during assembly, or invisible internal cracks from manufacturing, will gradually propagate under high heat and finally lead to end damage and breakage.
Contact me:Email:wp@cnjingganrefractory.com/sdwenping@163.com